Hydroxypropyl Cellulose
If you find any inaccurate information, please let us know by providing your feedback here

This article is compiled based on the United States Pharmacopeia (USP) – 2025 Edition
Issued and maintained by the United States Pharmacopeial Convention (USP)
Average molecular weight approximately 100,000 CAS RN®: 9004-64-2.
Viscosity: Dissolve 5.0 g of Hydroxypropyl Cellulose with 95.0 mL of water by stirring. If necessary, centrifuge the solution to expel any entrapped air bubbles. Determine the viscosity of the solution as directed in Viscosity—Rotational Methods 〈912〉 at 25 ± 0.1°. The viscosity is between 75 and 150 centipoises.